CÔNG THỨC KEM FOUNDATION CAO ẨM

CÔNG THỨC KEM FOUNDATION CAO ẨM

MOISTURIZING LIQUID FOUNDATION

STT
Tên nguyên liệu
INCI (tên hóa học)% sử dụng% sử dụng 
1KSG-310*PEG-15/Lauryl Dimethicone Crosspolymer
Mineral Oil
10.005.000 
2KF-6048*Polyglyceryl-3 Polydimethylsiloxyethyl Dimethicone2.001.000 
3KSG-16*Dimethicone/Vinyl Dimethicone Crosspolymer
Dimethicone
               4.002.000 
4KF-995*Cyclopentasiloxane               6.003.000 
5Ethylhexyl MethoxycinnamateEthylhexyl Methoxycinnamate3.001.500 
6KF96-6cs*Dimethicone4.702.350 
7KF-56A*Diphenylsiloxy Phenyl Trimethicone              5.002.500 
8KF-6028*Lauryl PEG-9 Polydimethylsiloxyethyl Dimethicone2.001.000 
9BS-MIX*PEG-10 Dimethicone
Cyclopentasiloxane
Quaternium 90 Bentonite
               5.002.500 
10PhenoxyethanolPhenoxyethanol0.400.200 
11Butylene GlycolButylene Glycol3.701.850 
12glyceringlycerin2.001.000 
13Sodium CitrateSodium Citrate0.300.150 
14Sodium ChlorideSodium Chloride0.100.050 
15WaterWater20.0010.000 
16TC powder/Bột TC * 15.007.500 
17KF-995*Cyclopentasiloxane               7.003.500 
18KF96-6cs*Dimethicone4.802.400 
19Sorbitan IsostearateSorbitan Isostearate4.002.000 
20KF-6106*Polyglyceryl-3 Polydimethylsiloxyethyl Dimethicone1.000.500 
   100.0050.000 
      
Phương pháp điều chế:    
      
 1. Phase A: Cân nguyên liệu 1 đến 9 và khuấy trong máy khuấy.
 2. Phase B: Cân nguyên liệu 10 đến 15 và trộn đều. 
 3. Phase C: Cân nguyên liệu 16 đến 20 và trộn bằng máy khuấy.
 4. Khi khuấy hôn hợp A trong máy khuấy  (khoảng 4,000rpm) thì cho Phase B vào từ từ và nhũ hóa. 
 5. Sau khi nhũ hóa, cho hỗn hợp C vào và khuấy đều để đồng nhất hỗn hợp. 
 6. Khuấy nhẹ (khoảng 2,000rpm) trong 1 phút để thu được sản phẩm.
* Chúng tôi có cung cấp các loại nguyên liệu này.